It is colour less liquid, odour similar to that of bergamot oil and french lavender. It os soluble in alcohol and ether. It is used in cosmetics and pharmaceutical cream preparations, other uses include softening agent, in toilet soap manufacturing , as a rust preventive, in cutting oils and in lubricants.
Market Position :
At present various small scale unites are manufacturing lanolin anhydrous beside seven/ eight big units. Because of its numerous and uses there is good scope to manufacturing this product.
Requirement Raw Material :
1. Lanolin ( crude ) 2000 kgs.
2. Bleaching Powder. 600 kgs.
3. Solvent ( Carbon tetra chloride) 400 Litters.
Manufacturing Process :
Crude wool grease is treated with alkali to remove free acid present and washed with water to remove excess of alkali. Neutral fat is treated with hydrogen peroxide and other bleaching agents. Next water and lanolin are separated form each other dy the use of selective solvents like carbon tetrachloride , alcohol etc.
Finally the product is checked for thermal cracking, ash , melting point, saponification value , iodine value, free acidity and colour.
Plant and machinery :
1. Steam jacketed (M.S) 1no.
2. Stainless steels solvent recovery tank. 1 no.
3. Mini Boiler 100 kgs/ hr. at a pressure of 150 psi 1 no.
4. Steam jacketed bleaching tank. 1 no.
5. Weighing scale 1 no.
6. Fire Extinguisher. 1 no.
7. Miscellaneous tools and equipments.
8. Stainless steel centrifuge 20" dia . with motor. 1 no.
9. Stainless still vat capacity 100 litters 1 no.
Introduction :
It is colour less liquid, odour similar to that of bergamot oil and french lavender. It os soluble in alcohol and ether. It is used in cosmetics and pharmaceutical cream preparations, other uses include softening agent, in toilet soap manufacturing , as a rust preventive, in cutting oils and in lubricants.
Market Position :
At present various small scale unites are manufacturing lanolin anhydrous beside seven/ eight big units. Because of its numerous and uses there is good scope to manufacturing this product.
Requirement Raw Material :
1. Lanolin ( crude ) 2000 kgs.
2. Bleaching Powder. 600 kgs.
3. Solvent ( Carbon tetra chloride) 400 Litters.
Manufacturing Process :
Crude wool grease is treated with alkali to remove free acid present and washed with water to remove excess of alkali. Neutral fat is treated with hydrogen peroxide and other bleaching agents. Next water and lanolin are separated form each other dy the use of selective solvents like carbon tetrachloride , alcohol etc.
Finally the product is checked for thermal cracking, ash , melting point, saponification value , iodine value, free acidity and colour.
Plant and machinery :
1. Steam jacketed (M.S) 1no.
2. Stainless steels solvent recovery tank. 1 no.
3. Mini Boiler 100 kgs/ hr. at a pressure of 150 psi 1 no.
4. Steam jacketed bleaching tank. 1 no.
5. Weighing scale 1 no.
6. Fire Extinguisher. 1 no.
7. Miscellaneous tools and equipments.
8. Stainless steel centrifuge 20" dia . with motor. 1 no.
9. Stainless still vat capacity 100 litters 1 no.